| MIL-I-12822C(MU)
each major defect and an AQL of 0.65 percent for each minor
defect. Equipment necessay for the performance of the inspec-
tions listed shall be in accordance with 4.3.4.
4.3.2.1 Retainer relay (dwg. 7548452)
Defects
Method, of
Categories
Code No.
Inspection
(see 6.2)
None defined.
Critical:
Major:
None defined.
AQL 2.50 percent
Minor:
Length...................... Gage
201
01001
202
Outside diameter............. Gage
01002
Split or crack in aluminum...... Visual
203
01003
Shellac missing.............. Visual
205
01005
Evidence of poor workmanship.. Visual
206
01006
4.3.2.2 Retainer relay assembly (dwg. 7543451)
Code No.
Categories
Defects
Method of
Inspection
Critical:
None defined.
Major:
None defined
Minor:
AQL 1.50 percent
201.
Disc improperly assembled....Visual
02001
02002
202.
Disc perforation missing.....Visual
Shellac on outer surface of
203.
disc..................... Visual
02003
4.3.2.3
Delay Element Assembly (dwg. 9209521)
Categories
Defects
Method of
Code No.
Inspection
Critical:
None defined.
Major:
AQL 100 percent
Primer paste missing......... Visual
101.
03001
Minor:
None defined.
6
|