| ![]() MIL-S-20517H(AR)
See Note.
4.4.3
Testing.
NOTE: Chemical Sampling. Representative samples of the components
identified in 4.4.3.1 shall be obtained in accordance with ASTM
procedure E300 for solids.
4.4.3.1 Moisture determination, Moisture determinations shall
be performed on the components specified in Table II.
MOISTURE DETERMINATION
TABLE II.
Requirement
Test Method
Components
Paragraph
Paraqraph
The contractor shall provide adequate controls to assure that
the materials comply with the requirements. For verification, the
contractor shall select and subject to test, one sample of each
material from each eight (8) hours production. A composite sample
shall not be used. If the moisture content of the sample exceeds
the requirement, that quantity or sub-lot of material represented by
the sample shall not be used in production. If the quantity of
material or sub-lot with excessive moisture has been used in loading
and packing, the remaining unloaded and unpacked material shall not
be used in production, and the loaded and packed simulators shall be
rejected. Test shall be performed as specified in 4.5.1.
(see dwg. 8848484). Major
4.4.3.2
Compressive tube strength
defects.
4.4.3.2.1 Axial. Thirteen (13) tubes shall be selected from
each lot for test. If one or more tubes fail to comply with the
requirement, the lot shall be rejected. The test shall be performed
as specified in 4.5.2.1 using equipment in accordance with 4.4.4.
(Destructive test)
4.4.3.2.2 Diametrical. Thirteen (13) tubes shall be selected
from each lot for test. If one or more tubes fail to comply with
the requirement, the lot shall be rejected. The test shall be
performed as specified in 4.5.2.2 using equipment in accordance with
4.4.4. (Destructive test)
31
|
Privacy Statement - Press Release - Copyright Information. - Contact Us |